Aluminum parts need to be protected. While natural oxidation does occur on aluminum if it’s not treated, it’s not sufficient or aesthetically pleasing enough for heavy-duty applications. Chromate conversion coating is one option for aluminum surface treatment, and anodizing is another. Both adhere a protective coating, both prevent corrosion – but they do so in completely different fashions and for different reasons.
How Each Process Actually Works
Chromate conversion coating is a chemical reaction with the aluminum surface that creates a thin protective layer. The part is immersed into a chromate solution and a chemical reaction occurs to turn the surface into a complex oxide coating. It takes place at room temperature within minutes, and it essentially becomes bonded into the surface of the metal (rather than on top).
In comparison, anodizing occurs through the application of an electrical current which builds up an oxide layer. In an electrolytic bath (usually sulfuric acid), the aluminum part becomes the anode. When electricity flows, oxidation occurs in a controlled fashion to create a porous oxide layer. This oxide layer is much thicker than naturally-occurring oxidation over time. This process takes an hour or longer depending on how much coating is desired.
The difference, fundamentally, is that chromate conversion creates a very thin coating through a chemical reaction while anodizing creates a much thicker layer through electrochemical oxidation.
Coating Thickness and Appearance
Coating thickness is where the significant differences come into play. Chromate conversion measurements range from 0.00001 – 0.0001 inches in thickness of the coating. It’s extremely thin – and so thin that measurement of part dimensions are unaffected. For precision manufacturing where even minimal dimensional changes cause problems, chromate conversion coating provides protection without adding thickness that would push parts out of specification.
In contrast, anodizing can create .0001 inch thickness or more (0.001). That’s 10-100 times thicker than chromate conversion. Parts already at the top of their toleranced allowance would go out of spec after anodizing if they needed something as minor as 0.001 inches added to them to begin with.
Appearance matters too; chromate conversion comes in various colors (clear, gold (iridescent), olive drab) but there is no evidence to suggest that one color is thicker, better, more corrosive – instead, they all speak to different processes within the chromate realm. Anodizing can remain as natural silver-gray coloring, can be dyed any color (the process takes more work however), or can take on a dark bronze appearance (through certain electrolytes).
Corrosion Protection Performance
Both coatings protect against corrosion but in different fashions. Chromate conversion provides good corrosion resistance through its chemical nature, for example. Chromate itself is naturally an anti-corrosive agent and has some self-healing properties – if it gets scratched off, it can migrate to protect those areas that were exposed.
Anodizing limits aluminum exposure to the atmosphere; the thicker the oxide layer, the better protection it provides. Hard anodizing (Type III) has excellent corrosion protection in extreme environments, while standard sulfuric anodizing (Type II) has good corrosion resistance in most cases.
However, unsealed anodized items often corrode faster than bare aluminum under certain environmental conditions; sealing helps.
Surface Preparation and Paint Adhesion
This is where the advantage always goes to chromate conversion. The results of such treatment are ideal for paint adhesion and other organic coatings for combined protective solutions for further durability. Paint sticks well enough to anodizing surfaces, but not as well as chromate-treated surfaces. This is why chromate conversion is often desired as an industry standard for any painting solution after the fact (especially in aerospace and military operations).
In certain situations where surfaces are supposed to be painted, anodizing makes little sense. However, anodized surfaces are certainly preferred when their durability and aesthetic appeal serve a purpose without paint.
Cost and Processing Time
Chromate conversion is often cheaper and quicker; it works at room temperature in a matter of minutes; it avoids electrical connections needing to be maintained by an operator; racking setups are easier and equipment complications are much less than anodizing systems.
Anodizing is more expensive and time consuming; it requires temperature-controlled baths for proper operation; electrical controls must be maintained; immersion times increase as do potential additional finishing steps like sealing; equipment investment is higher and energy costs are greater.
But sometimes anodizing just makes sense for the additional costs – even for high-volume production runs. If a specific part requires certain qualities that only anodizing provides, it doesn’t always make sense to go with the cheaper option; it needs to meet requirements.
Wear Resistance and Hardness
This is another case where anodizing proves dominant – anodized hard surfaces are much harder than metal systems created from original aluminum; anodized finishes get super hard with application – harder than most tool steels – as it’s applied with an increased current.
Chromate conversion does not lend itself to hardness; it does not increase surface hardness nor does it treat portions thin enough to make significant wear resistance of any merit.
Thus surfaces exposed to wear should be anodized – surfaces that will have a paint finish need chromate conversion.
Electrical Conductivity Considerations
Chromate conversion retains good electrical conductivity; chipping through does not compromise connectivity sufficiently enough to make a difference between caution during connection points; where grounding needs exist or other electronic circumstances do rely on conductivity, chromate conversion works best.
Anodizing raises an insulative level; anodized parts will not promote conductivity as designed at anodized points. If parts need electrical connection after they’re created, those areas must have been masked during the process or coating thereafter must have occurred.
Thus for electrics and electronics situations where both conductive connectivity and protection are needed, chromate conversion makes more sense here as well.
Meeting Specifications and Standards
Both processes rely on industry standards and military specifications for understanding what will work best. MIL-DTL-5541 covers chromate conversion systems while MIL-A-8625 covers anodizing specifications.
Each has their types and classes depending on what’s specifically required.
To meet specifications requires common processing control methods as well as testing and documentation. Not all finishing companies can do both procedures effectively – some specialize in one or none – but knowing what your application needs helps determine a viable supplier who also meets standards.
Making the Right Choice
Ultimately, choosing between two processes depends on application needs – the environment in which it’ll experience excess use; whether it needs paint down the road; whether there’s toleranced concerns; whether wear resistance plays into quality control efforts; whether specifications recommend one over another.
Chromate conversion works best when parts will need paint down the road to increase adhesion effectiveness, or when tight toleranced success need addressing, or when conductivity matters for effective corrosion prevention systems.
Anodizing works better when strict treatment for toughness and aesthetic appeal occurs without paint down the road, when wear resistance must be proven effective due to applied action stressors, or when excessive treatment matters but cost does not play an issue.
Sometimes the processes can be used concurrently – some applications have anodizing done first and then add chromate treatment before paints go on.
But this won’t happen unless people know what’s best by learning how each process truly does not protect but instead protects aluminum in drastically different fashions.Getting behind what each one actually does instead of assuming they both protect goes a long way in determining the best possible surface treatment for applications that matter specifically to you.